VJ....31X RoHS Automotive MLCC
www.vishay.com
Vishay Vitramon
Revision: 29-May-18
16
Document Number: 45226
For technical questions, contact: mlcc@vishay.com
THIS DOCUMENT IS SUBJECT TO CHANGE WITHOUT NOTICE. THE PRODUCTS DESCRIBED HEREIN AND THIS DOCUMENT
ARE SUBJECT TO SPECIFIC DISCLAIMERS, SET FORTH AT www.vishay.com/doc?91000
5 - INSPECTION CRITERIA
The supplier shall carry out visual examination with suitable equipment with approximately 10 x magnification and lighting
appropriate to the specimen under test and the required quality level.
Chipping
The components shall be free of cracks or fissures. Small damages which do not deteriorate the performance of the component
shall be less than 50 % of the surface of the MLCC as defined in EIA 595.
Delamination or Exposed Electrodes
No visible separation or delamination between layers of the capacitor and no exposed electrodes between the two terminals of
the capacitor must be seen.
Metallization
For the metallization, no visible detachment of the metallized terminals and no exposed electrodes must be seen. Defects and
gaps in the metallization on each sides of the terminal must not exceed 10 % of the total area (e.g. A, B, C, …). Leaching shall
not exceed 25 %.
Electrode Distance
The ceramic body shall be free of any conducting material between the terminals which reduces the distance of the electrodes.
The minimum distance “D” is 400 μm for all package sizes, except 0402. For the component package 0402 the minimum
distance is 200 μm.
C
A
B
D