17-21SURC/S530-A3/TR8

EVERLIGHT ELECTRONICS CO., LTD.
17-21SURC/S530-A3/TR8
Everlight Electronics Co., Ltd. http://www.everlight.com Rev.: 1 Page: 7 of 9
Device No: SZDSE-171- Prepared date: 7-Apr.-2009 Prepared by: Huang yongxin
Reliability Test Items And Conditions
The reliability of products shall be satisfied with items listed below.
Confidence level90%
LTPD10%
No. Items Test Condition
Test
Hours/Cycles
Sample
Size
Ac/Re
1 Reflow Soldering
Temp. : 260℃±5
Min. 5sec.
6 Min.
22 PCS. 0/1
2 Temperature Cycle
H : +100 15min
5 min
L : -40 15min
300 Cycles
22 PCS. 0/1
3 Thermal Shock
H : +100 5min
10 sec
L : -10 5min
300 Cycles
22 PCS. 0/1
4
High Temperature
Storage
Temp. : 100
1000 Hrs.
22 PCS. 0/1
5
Low Temperature
Storage
Temp. : -40
1000 Hrs.
22 PCS. 0/1
6 DC Operating Life IF = 20 mA
1000 Hrs.
22 PCS. 0/1
7
High Temperature /
High Humidity
85/ 85%RH
1000 Hrs.
22 PCS. 0/1
EVERLIGHT ELECTRONICS CO., LTD.
17-21SURC/S530-A3/TR8
Everlight Electronics Co., Ltd. http://www.everlight.com Rev.: 1 Page: 8 of 9
Device No: SZDSE-171- Prepared date: 7-Apr.-2009 Prepared by: Huang yongxin
Precautions For Use
1. Over-current-proof
Customer must apply resistors for protection , otherwise slight voltage shift will cause big
current change ( Burn out will happen ).
2. Storage
2.1 Do not open moisture proof bag before the products are ready to use.
2.2 Before opening the package: The LEDs should be kept at 30 or less and 90%RH or less.
2.3 After opening the package: The LED's floor life is 1 year under 30 or less and 60% RH or less.
If unused LEDs remain, it should be stored in moisture proof packages.
2.4 If the moisture absorbent material (silica gel) has faded away or the LEDs have exceeded the
storage time, baking treatment should be performed using the following conditions.
Baking treatment : 60±5 for 24 hours.
3. Soldering Condition
3.1 Pb-free solder temperature profile
3.2 Reflow soldering should not be done more than two times.
3.3 When soldering, do not put stress on the LEDs during heating.
3.4 After soldering, do not warp the circuit board.
EVERLIGHT ELECTRONICS CO., LTD.
17-21SURC/S530-A3/TR8
Everlight Electronics Co., Ltd. http://www.everlight.com Rev.: 1 Page: 9 of 9
Device No: SZDSE-171- Prepared date: 7-Apr.-2009 Prepared by: Huang yongxin
4.Soldering Iron
Each terminal is to go to the tip of soldering iron temperature less than 350 for 3 seconds
within once in less than the soldering iron capacity 25W. Leave two seconds and more intervals, and do
soldering of each terminal. Be careful because the damage of the product is often started at the time of
the hand solder.
5.Repairing
Repair should not be done after the LEDs have been soldered. When repairing is unavoidable, a
double-head soldering iron should be used (as below figure). It should be confirmed beforehand whether
the characteristics of the LEDs will or will not be damaged by repairing.
EVERLIGHT ELECTRONICS CO., LTD. Tel: 886-2-2267-2000, 2267-9936
Office: No 25, Lane 76, Sec 3, Chung Yang Rd, Fax: 886-2267-6244, 2267-6189, 2267-6306
Tucheng, Taipei 236, Taiwan, R.O.C http://www.everlight.com

17-21SURC/S530-A3/TR8

Mfr. #:
Manufacturer:
Everlight
Description:
Standard LEDs - SMD Red, 624nm 60mcd, 20mA
Lifecycle:
New from this manufacturer.
Delivery:
DHL FedEx Ups TNT EMS
Payment:
T/T Paypal Visa MoneyGram Western Union

Products related to this Datasheet