TLP290(SE
Soldering and Storage
1. Soldering
1.1 Soldering
When using a soldering iron or medium infrared ray/hot air reflow, avoid a rise in device temperature as
much as possible by observing the following conditions.
1) Using solder reflow
·Temperature profile example of lead (Pb) solder
·Temperature profile example of using lead (Pb)-free solder
Reflow soldering must be performed once or twice.
Time (s)
(°C)
240
210
160
60 to 120s
less than 30s
Package surface temperature
140
Time
This profile is based on the device’s
maximum heat resistance guaranteed
value.
Set the preheat temperature/heating
temperature to the optimum temperature
corresponding to the solder paste
type used by the customer within the
described profile.
This profile is based on the device’s
maximum heat resistance guaranteed
value.
Set the preheat temperature/heating
temperature to the optimum temperature
corresponding to the solder paste
type used by the customer within the
described profile.
(°C)
260
230
190
60 to 120s
30 to 50s
180
Package surface temperature
(s)
The mounting shoul
d be completed with the interval from the first to the last mountings being 2 weeks.
2) Using solder flow (for lead (Pb) solder, or lead (Pb)-free solder)
・Please preheat it at 150°C between 60 and 120 seconds.
・Complete soldering within 10 seconds below 260°C. Each pin may be heated at most once.
3) Using a soldering iron
Complete soldering within 10 seconds below 260°C, or within 3 seconds at 350°C. Each pin may
be heated at most once.
2013-05-27